Monday, 27 February 2012

Keel stripping

It's impossible to take paint/ antifoul off a metal keel with a heat gun, and sanding more that one layer of paint takes a long time. I had some nitromors at home, so I took that along and finished off the tin on the keel. It's still not down to bare metal, but it's not nearly as lumpy as it was!

The varnol I put on on Friday looks good, so I finished preparing the cabin sides. The day is too damp to put any more varnol on though, so I came home early.